WT 50Ni2 – BAg-24 Silver

…/ 763°C Brazing Temperature Range Low: 1355°F / 735°C Liquidus: 1305°F / 707°C Solidus: 1220°F / 660°C Chemical Composition: Ag Cu Zn Ni 50% 20% 28% 2% View/Download Data Sheet0ni2…

Read more
Mangweld 44 – Hardfacing Electrode and Wire

…Parameters: Diameter: 1/8” 5/32” 3/16” Current: DCRP DCRP DCRP Amperage: 125-140 140-160 175-200 Chemical Composition: C Mn Si Cr Ni Fe 0.3 16.0 0.3 15.0 0.5 BAL View/Download Data Sheet…

Read more
WT 4130VM

…Room Temp Tensile Strength (PSI): 120,000-140,000 Approx. Tempering Temp (°F): 925; Room Temp Tensile Strength (PSI): 140,000-160,000 Approx. Tempering Temp (°F): 725; Room Temp Tensile Strength (PSI): 180,000-200,000 Typical Chemical…

Read more
ER 2553 – Stainless Steel Welding Wire

…diameters in spool and wire rods. Chemical Composition (Wt%): Si Mn Cu Mo S Ni Cr P C 1.0 1.5 1.5-2.5 2.9-3.9 0.03 4.5-6.5 24.0-27.0 0.04 0.04 View/Download Data Sheet…

Read more
WT 23-99

…Strength: 36-50 ksi Elongation in 2”: 6-12 Reduction of area: 20 Chemical Composition (Wt%): C Mn Si S Fe N Cu 1.0 2.5 0.75 0.03 4.0 90 min. 4.0 Note:…

Read more
ER317/317L – Stainless Steel Welding Wire

…(Wt%): Si Mn Cu Mo S Ni Cr P C 0.30-0.65 1.0-2.5 0.75 3.0-4.0 0.03 13.0-15.0 18.5-20.5 0.03 0.03 Note: Single values are maximum unless otherwise noted. View/Download Data Sheet…

Read more
Weldman 1 – Hardfacing Electrode

Parameters: Diameter: 1/8” 5/32” 3/16” 1/4″ Current: DCRP DCRP DCRP DCRP Amperage: 125-140 140-160 175-200 200-250 Characteristics: Deposit Layers: Multiple Machinability: Poor Hardness as deposited: 15-22 Work Hardened: 45-50 Tensile…

Read more
ER347 – Stainless Steel Welding Wire

…Nb + Ta 0.30-0.65 1.0-2.5 0.75 0.75 0.03 9.0-11.0 19.0-21.5 0.03 0.08 (10 x C) min – 1.0 max Note: Single values are maximum unless otherwise noted. View/Download Data Sheet…

Read more
ER321 – Stainless Steel Welding Wire

…P C Ti 0.30-0.65 1.0-2.5 0.75 0.75 0.03 9.0-11.0 18.5-20.5 0.03 0.08 (9 x C) min – 1.0 max Note: Single values are maximum unless otherwise noted. View/Download Data Sheet…

Read more
Titanium Grade 7 – ERTi-7

…in wire and spool. Chemical Composition (Wt%): Fe O C N H Ti Pd 0.12 0.08-0.16 0.03 0.015 0.008 BAL 0.12-0.25 Note: Single values are maximum unless otherwise noted. View/Download

Read more